Material Density Reference
Use grade-specific values with their conditions. This compact reference deliberately leaves unsourced properties blank.
| Material | Density kg/m³ | Conductivity W/(m·K) | Specific heat J/(kg·K) | Conditions & source |
|---|---|---|---|---|
| Copper C11000 (ETP) | 8,920 | 394 | Not supplied | Copper Development Association design guide; nominal physical values. Conductivity is a rounded guide value, not an acceptance limit. CDA copper-alloy design guide |
| TECAFORM AH natural (POM-C) | 1,410 | 0.39 | 1,400 | Unfilled stock shape. CLTE is longitudinal, 23–60 °C. Conductivity and heat capacity: ISO 22007-4. Typical data, not a specification. Ensinger product data |
| BISCO HT-800 silicone foam | 352 | 0.076 | Not supplied | Medium cellular silicone, typical density 22 lb/ft³. Thermal conductivity 0.076 W/(m·K), ASTM C518. Foam is not interchangeable with solid silicone. Rogers HT-800 technical data sheet |
Density is a measured material property
A family label such as metal, polymer or rubber does not identify one density. For a known specimen, calculate density from measured mass and volume. For a design estimate, identify the grade and condition before using a table value.
Use the values together carefully
Thermal diffusivity is k/(ρcp), with compatible conductivity, density and heat-capacity values. Do not combine numbers from unrelated grades to fill a missing cell. When conditions are incompatible, report the result as unavailable until suitable data are obtained.
For a first mass estimate, m = ρV. Volume uncertainty and porosity may matter more than an extra decimal place in the tabulated density.
Compare the sourced materials →